Chapter 6.2: Stress Rupture Failures
-
Published:2018
Abstract
Boiler tubes operating at high temperatures under significant pressure are vulnerable to stress rupture failures. This chapter examines the cause, effect, and appearance of such failures. It discusses the conditions and mechanisms that either lead to or are associated with stress rupture, including overheating, high-temperature creep, graphitization, and dissimilar metal welds. It explains how to determine which mechanisms are in play by interpreting fracture patterns and microstructural details. It also describes the investigation of several carbon and low-alloy steel tubes that failed due to stress rupture.
Stress Rupture Failures, Failure Investigation of Boiler Tubes: A Comprehensive Approach, By Paresh Haribhakti, P.B. Joshi, Rajendra Kumar, ASM International, 2018, p 149–204, https://doi.org/10.31399/asm.tb.fibtca.t52430149
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.