Failure Investigation of Boiler Tubes: A Comprehensive Approach
Chapter 3: Metallurgy of Steels and Related Boiler Tube Materials
-
Published:2018
Abstract
This chapter describes the metallurgy, composition, and properties of steels and other alloys. It provides information on the atomic structure of metals, the nature of alloy phases, and the mechanisms involved in phase transformations, including time-temperature effects and the role of diffusion, nucleation, and growth. It also discusses alloying, heat treating, and defect formation and briefly covers condenser tube materials.
Sign in
ASM members
Member Sign InMetallurgy of Steels and Related Boiler Tube Materials, Failure Investigation of Boiler Tubes: A Comprehensive Approach, By Paresh Haribhakti, P.B. Joshi, Rajendra Kumar, ASM International, 2018, p 27–86, https://doi.org/10.31399/asm.tb.fibtca.t52430027
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!