Corrosion: Understanding the Basics
Chapter 10: Corrosion Control by Cathodic and Anodic Protection
-
Published:2000
Abstract
This article describes in detail the process of corrosion control by cathodic and anodic protection. The discussion covers the basic concept of cathodic and anodic protection systems, their types and equipment used, and the advantages, limitations, and applications of these protection systems. The types of cathodic protection systems include sacrificial cathodic protection and impressed-current cathodic protection systems. Some of the technical problems associated with cathodic protection include the effects of stray currents on the corrosion of adjacent metal structures, the effects of the chemical reactions occurring at the surface of the protected structure, and the effects of cathodic protection on coatings.
Corrosion Control by Cathodic and Anodic Protection, Corrosion: Understanding the Basics, Edited By J.R. Davis, ASM International, 2000, p 407–426, https://doi.org/10.31399/asm.tb.cub.t66910407
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!