Microelectronics Failure Analysis: Desk Reference (Seventh Edition)
Failure Analysis Techniques and Methods for Microelectromechanical Systems (MEMS)[1]
-
Published:2019
Abstract
This chapter discusses the various failure analysis techniques for microelectromechanical systems (MEMS), focusing on conventional semiconductor manufacturing processes and materials. The discussion begins with a section describing the advances in integration and packaging technologies that have helped drive the further proliferation of MEMS devices in the marketplace. It then shows some examples of the top MEMS applications and quickly discusses the fundamentals of their workings. The next section describes common failure mechanisms along with techniques and challenges in identifying them. The chapter also provides information on the testing of MEMS devices. It covers the two common challenges in sample...
Sign in
ASM members
Member Sign InDavid E. Grosjean, Failure Analysis Techniques and Methods for Microelectromechanical Systems (MEMS), Microelectronics Failure Analysis: Desk Reference, 7th ed., Edited By Tejinder Gandhi, ASM International, 2019, p 563–586, https://doi.org/10.31399/asm.tb.mfadr7.t91110563
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.