Chapter 27: Physical Properties
-
Published:1995
Abstract
This chapter describes the physical properties of steels used for castings. The properties covered include density, modulus of elasticity, Poisson's ratio, shear modulus, thermal expansion, thermal conductivity, specific heat, thermal diffusivity, electrical resistivity, and magnetic properties.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Physical Properties, Steel Castings Handbook, 6th ed., Edited By Malcolm Blair, Thomas L. Stevens, ASM International, 1995, p 27-1–27-17, https://doi.org/10.31399/asm.tb.sch6.t68200404
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Thermal Conductivity and Thermal Diffusivity
Materials at Low Temperatures
Electromagnetic and Thermal Properties of Materials
Induction Heating and Heat Treatment
Thermomechanical Testing
Metalworking: Bulk Forming
Thermal Analysis and Thermal Properties
Characterization and Failure Analysis of Plastics
Physical and Mechanical Properties of Select Alloys
Stainless Steels for Design Engineers
Lamina and Laminate Nonmechanical Testing
Composites
Physical Properties of Cast Irons
Cast Iron Science and Technology
Workpiece Materials Database
Metalworking: Bulk Forming
Theory of Heating by Induction
Practical Induction Heat Treating (Second Edition)
Thermal Properties of Carbon and Low-Alloy Steels
Heat Treating of Irons and Steels