Chapter 17: Quality Control and Quality Assurance
-
Published:1995
Abstract
Casting quality and consistency need to be carefully controlled. This chapter discusses the procedures that describe the process and product quality controls. In addition, it provides information on quality assurance programs.
You do not currently have access to this chapter.
Citation
Quality Control and Quality Assurance, Steel Castings Handbook, 6th ed., Edited By Malcolm Blair, Thomas L. Stevens, ASM International, 1995, p 17-1–17-12, https://doi.org/10.31399/asm.tb.sch6.t68200220
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.
Related Book Content
Overview of Quality and the Standards, Programs, and Certifications Used in the Coatings Industry
Protective Organic Coatings
Introduction to Steel Castings
Steel Castings Handbook (Sixth Edition)
Industrial Applications of Steel Castings
Steel Castings Handbook (Sixth Edition)
Purchasing Policy
Steel Castings Handbook (Sixth Edition)
Advantages of Steel Castings
Steel Castings Handbook (Sixth Edition)
Casting Alloys
Stainless Steels for Design Engineers
Process Capability and Tolerances
Steel Castings Handbook (Sixth Edition)
Cast-Weld Construction
Steel Castings Handbook (Sixth Edition)
Finishing, Heat Treatment and Inspection
Steel Castings Handbook (Sixth Edition)