Abstract
This chapter explains various aspects of the foundry process that the design engineer should consider when designing steel castings. It discusses special feeding aids, such as tapers, padding, ribs, and chills that may be used by foundry personnel to promote directional solidification. The chapter addresses the design of castings to reduce the occurrence of internal shrinkage. It provides a detailed discussion on design considerations for molding, cleaning, machining, and function.
Manufacturing Design Considerations, Steel Castings Handbook, 6th ed., Edited By Malcolm Blair, Thomas L. Stevens, ASM International, 1995, p 7-1–7-17, https://doi.org/10.31399/asm.tb.sch6.t68200115