Book Chapter
Chapter 1: Introduction to Steel Castings
-
Published:1995
Abstract
This chapter defines steel castings, explains when to use steel castings, gives an overview of casting processes, and gives examples of suitable applications for cast steel parts.
You do not currently have access to this chapter.
Citation
Introduction to Steel Castings, Steel Castings Handbook, 6th ed., Edited By Malcolm Blair, Thomas L. Stevens, ASM International, 1995, p 1-1–1-5, https://doi.org/10.31399/asm.tb.sch6.t68200001
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Industrial Applications of Steel Castings
Steel Castings Handbook (Sixth Edition)
Purchasing Policy
Steel Castings Handbook (Sixth Edition)
Casting Alloys
Stainless Steels for Design Engineers
Quality Control and Quality Assurance
Steel Castings Handbook (Sixth Edition)
Advantages of Steel Castings
Steel Castings Handbook (Sixth Edition)
Process Capability and Tolerances
Steel Castings Handbook (Sixth Edition)
Cast-Weld Construction
Steel Castings Handbook (Sixth Edition)
Finishing, Heat Treatment and Inspection
Steel Castings Handbook (Sixth Edition)
Specifying Steel Castings
Steel Castings Handbook (Sixth Edition)