Tool Steels (Fifth Edition)
Chapter 17: Troubleshooting: Manufacturing and Performance Problems
-
Published:1998
Abstract
This chapter presents an overview of some of the major causes of tool and die failures. The chapter describes fracture and fracture toughness of tool steels, and the influence of factors such as steel quality and primary processing, mechanical design, heat treatment, grinding and finishing, and distortion and dimensional change.
Troubleshooting: Manufacturing and Performance Problems, Tool Steels, 5th ed., By George Roberts, George Krauss, Richard Kennedy, ASM International, 1998, p 325–343, https://doi.org/10.31399/asm.tb.ts5.t65900325