The low-alloy special-purpose tool steels, designated as group L steels in the AISI classification system, are similar to the water-hardening tool steels but have somewhat greater alloy content. This chapter discusses the metallurgy and performance of low-alloy special-purpose tool steels, including those with high carbon content, those with medium carbon content, and those containing nickel.
Low-Alloy Special-Purpose Tool Steels, Tool Steels, 5th ed., By George Roberts, George Krauss, Richard Kennedy, ASM International, 1998, p 141–163, https://doi.org/10.31399/asm.tb.ts5.t65900141