Chapter 1: Introduction—An Overview of Microstructure in Materials
-
Published:2008
Abstract
This chapter explains the distinction between materials and matter through the concept of microstructure. It presents the history of matter science and the establishment of metallography. The chapter provides an overview of the progress of steel technology, progress in synthetic polymers and ceramics, and establishment and development of materials science.
You do not currently have access to this chapter.
Citation
Introduction—An Overview of Microstructure in Materials, Thermodynamics of Microstructures, By Taiji Nishizawa, ASM International, 2008, p 1–12, https://doi.org/10.31399/asm.tb.tm.t52320001
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.
Related Book Content
Introduction to Steels and Cast Irons
Metallographer’s Guide Practices and Procedures for Irons and Steels
Glossary of Terms: Metallography and Microstructure
Metallography and Microstructures
Abbreviations and Symbols: Metallography and Microstructure
Metallography and Microstructures
Solid Particle Erosion
Friction, Lubrication, and Wear Technology
Metallography of Titanium and Its Alloys
Titanium Physical Metallurgy, Processing, and Applications
Medical Device Materials Reference
Materials for Medical Devices
Nomenclature of Phases and Constituents
Light Microscopy of Carbon Steels
Image Analysis
Materials Characterization
Metallography of Archaeological Alloys
Metallography and Microstructures
Glossary
Metallographer’s Guide Practices and Procedures for Irons and Steels