Appendix 11: Cross-Reference to Steels
-
Published:1996
Abstract
This appendix contains a cross-reference to steels, which was developed to help the Heat Treater cross-index chemically similar specifications. The specifications are listed alpha-numerically by country of origin.
Topics
Steel
You do not currently have access to this chapter.
Citation
Cross-Reference to Steels, Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels, By Charlie R. Brooks, ASM International, 1996, p 418–430, https://doi.org/10.31399/asm.tb.phtpclas.t64560418
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.
Related Book Content
Introduction—Purpose of Text, Microstructure and Analysis, Steel Definitions, and Specifications
Steels: Processing, Structure, and Performance (Second Edition)
Steel as a Material
Metallography of Steels Interpretation of Structure and the Effects of Processing
AISI-SAE System of Designations for Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Steel Cross Reference to AISI/SAE Designations
Heat Treating of Irons and Steels
History and Primary Steel Processing
Steels: Processing, Structure, and Performance (Second Edition)
Steel Hardness Conversions
Metallurgy for the Non-Metallurgist (Second Edition)
Introduction
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Glossary of Terms: Surface Engineering
Surface Engineering
Nomenclature of Phases and Constituents
Light Microscopy of Carbon Steels
Temper Colors for Steels
Failure Analysis of Heat Treated Steel Components