This chapter provides information on the selection of steel and the design of its heat treatment. It also discusses the purpose of this book.
Topics
Carbon steel,
Low-alloy steel,
Structural steel,
Hardenability testing,
Precipitation hardening,
Annealing,
Austenitizing,
Normalizing,
Oil quenching,
Water quenching,
Austempering,
Martempering,
Tempering,
Chemical composition,
Rate of decomposition,
Hardenability,
Fracture toughness,
Hardness,
Plastic deformation properties,
Tensile properties,
Heat transfer properties,
Recrystallization temperature,
Steel,
Heat treatment
You do not currently have access to this chapter.
Citation
Introduction, Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels, By Charlie R. Brooks, ASM International, 1996, p 1–2, https://doi.org/10.31399/asm.tb.phtpclas.t64560001
Download citation file:
New Handbook: Volume 11B
Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.
Related Book Content
Decarburization of Steels
Practical Heat Treating (Second Edition)
Heat Treatment of Gears
Heat Treatment of Gears A Practical Guide for Engineers
Austenitizing and Typical Heat Treatment Temperatures for Steels
Heat Treating of Irons and Steels
The Various Microstructures of Room-Temperature Steel
Steel Metallurgy for the Non-Metallurgist
Origin of Microstructure
Metallographer’s Guide Practices and Procedures for Irons and Steels
The Metallographer and the Metallographic Laboratory
Metallographer’s Guide Practices and Procedures for Irons and Steels
Stress-Relief Heat Treating of Steel
Steel Heat Treating Fundamentals and Processes
Steel Heat Treating Process Control—An Introduction
Steel Heat Treating Technologies
Cleaning of Steel for Heat Treatment
Steel Heat Treating Fundamentals and Processes
Fundamentals of the Heat Treating of Steel
Practical Heat Treating (Second Edition)