Chapter 4: The Role of Materials in Defining Process Constraints
-
Published:2004
Abstract
This chapter considers the materials and processing aspects of soldering and the manner in which these interrelate in the development of joining processes. It discusses the processes involved in eliminating or suppressing metallurgical and mechanical constraints as well as constraints imposed by the components.
Topics
Soldering
You do not currently have access to this chapter.
Citation
The Role of Materials in Defining Process Constraints, Principles of Soldering, By Giles Humpston, David M. Jacobson, ASM International, 2004, p 145–187, https://doi.org/10.31399/asm.tb.ps.t62440145
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
The Role of Materials in Defining Process Constraints
Principles of Brazing
Selected References
Principles of Soldering
History
Principles of Soldering
Abbreviations and Symbols
Principles of Soldering
Induction Hardening for the Aeronautic and Aerospace Industry
Induction Heating and Heat Treatment
Introduction to Mechanical Testing of Components
Mechanical Testing and Evaluation
Fretting Wear Failures
Failure Analysis and Prevention (2021 Edition)
Hot Gas Soldering
Welding, Brazing, and Soldering
Introduction to Special Welding and Joining Topics
Welding, Brazing, and Soldering
Failures in Soldering
Analysis and Prevention of Component and Equipment Failures