Chapter 2: Solders and Their Metallurgy
-
Published:2004
Abstract
This chapter presents an overview and survey of solder alloy systems. Extensive reference is made to phase diagrams and their interpretation. The chapter describes the effect of metallic impurities on different solders. The chapter concludes with a review of the key characteristics of eutectic alloys and of the factors most effective at depressing the melting point of solders by eutectic alloying.
You do not currently have access to this chapter.
Citation
Solders and Their Metallurgy, Principles of Soldering, By Giles Humpston, David M. Jacobson, ASM International, 2004, p 49–102, https://doi.org/10.31399/asm.tb.ps.t62440049
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
History
Principles of Soldering
Phase Diagram Determination
Phase Diagrams Understanding the Basics
The Joining Environment
Principles of Soldering
Brazes and Their Metallurgy
Principles of Brazing
Isomorphous Alloy Systems
Phase Diagrams Understanding the Basics
Solutions and Phase Diagrams
Steel Metallurgy for the Non-Metallurgist
Understanding the Metallurgy of Titanium
Titanium: A Technical Guide (Second Edition)
Monotectic Alloy Systems
Phase Diagrams Understanding the Basics
Computer Simulation of Phase Diagrams
Phase Diagrams Understanding the Basics
Thermodynamics of Phase Diagrams
Thermodynamics of Microstructures