Chapter 10: Tensile Testing of Ceramics and Ceramic-Matrix Composites
-
Published:2004
Abstract
This chapter describes tensile testing of advanced ceramic materials, a category that includes both noncomposite, or monolithic, ceramics and ceramic-matrix composites (CMCs). The chapter presents four key considerations that must be considered when carrying out tensile tests on advanced monolithic ceramics and CMCs. These include effects of flaw type and location on tensile tests, separation of flaw populations, design strength and scale effects, and lifetime predictions and environmental effects. The chapter discusses the advantages, problems, and complications of four basic categories of tensile testing techniques as applied to ceramics and CMCs. These categories are true direct uniaxial tensile tests...
Sign in
ASM members
Member Sign InTensile Testing of Ceramics and Ceramic-Matrix Composites, Tensile Testing, 2nd ed., Edited By J.R. Davis, ASM International, 2004, p 163–182, https://doi.org/10.31399/asm.tb.tt2.t51060163
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field