Tensile Testing (Second Edition)
Chapter 8: Tensile Testing of Plastics
-
Published:2004
Abstract
The testing of plastics includes a wide variety of chemical, thermal, and mechanical tests. This chapter reviews the tensile testing of plastics, which has been standardized in ASTM D 638, "Standard Test Method for Tensile Properties of Plastics," and other comparable standards. It describes the fundamental factors that affect data from tensile tests, examines the stipulations in standardized tensile testing, and discusses the utilization of data from tensile tests.