Gear Materials, Properties, and Manufacture
Chapter 13: Gear Failure Modes and Analysis
-
Published:2005
Abstract
Gears can fail in many different ways, and except for an increase in noise level and vibration, there is often no indication of difficulty until total failure occurs. This chapter begins with the classification of gear failure modes, followed by sections discussing the characteristics of various fatigue failures. Then, it provides information on the modes of impact fractures, wear, scuffing, and stress rupture. Next, the chapter describes the causes of gear failures and discusses the processes involved in conducting the failure analysis. Finally, the chapter presents examples of gear failure analysis.
Gear Failure Modes and Analysis, Gear Materials, Properties, and Manufacture, Edited By J.R. Davis, ASM International, 2005, p 257–291, https://doi.org/10.31399/asm.tb.gmpm.t51250257
Download citation file:
New Handbook: Volume 11B
Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.