Fatigue and Durability of Structural Materials
Appendix: Selected Relevant Background Information
-
Published:2006
Abstract
This appendix provides supplemental information on the metallurgical aspects of atomic structure, the use of dislocation theory, heat treatment processes and procedures, important engineering materials and strengthening mechanisms, and the nature of elastic, plastic, and creep strain components. It also provides information on mechanical property and fatigue testing, the use of hysteresis energy to analyze fatigue, a procedure for inverting equations to solve for dependent variables, and a method for dealing with the statistical nature of failure.
Selected Relevant Background Information, Fatigue and Durability of Structural Materials, By S.S. Manson, G.R. Halford, ASM International, 2006, p 375–439, https://doi.org/10.31399/asm.tb.fdsm.t69870375