Data Set 5: Creep Rupture Properties
-
Published:2004
Abstract
This data set contains the results of uniaxial creep rupture tests for a wide range of aluminum casting alloys conducted at temperatures from 100 to 315 deg C. In most cases, tests were made of several lots of material of each alloy and temper, the results were analyzed, and the averages were normalized to the room-temperature typical values. For some alloys, "representative" values (raw data) rather than typical values are provided.