Data Set 3: Stress-Strain Curves
-
Published:2004
Abstract
The stress-strain curves in this data set are representative examples of the behavior of several cast alloys under tensile or compressive loads. The curves are arranged by alloy designation. Each figure cites the original source of the curve and provides pertinent background information as available. Compressive tangent modulus curves are presented for certain alloys. The effects of cyclic loading are given on several curves.
Topics
Microstructure,
Casting defects,
Rotating bend fatigue testing,
Corrosion-resistant alloys,
High-temperature alloys,
Cast aluminum alloys,
Aluminum alloys,
Expendable mold casting,
Filling and feeding,
Permanent mold casting,
Aging,
Annealing,
Quenching,
Solution heat treatment,
Alloy composition,
Creep properties,
Fatigue properties,
Fracture toughness,
Brinell hardness,
Stress-strain curves,
Tensile properties,
Viscoelastic properties,
Physical properties,
Thermal expansion,
Cast metal products
You do not currently have access to this chapter.
Citation
Stress-Strain Curves, Aluminum Alloy Castings: Properties, Processes, and Applications, By J. Gilbert Kaufman, Elwin L. Rooy, ASM International, 2004, p 193–209, https://doi.org/10.31399/asm.tb.aacppa.t51140193
Download citation file:
Related Book Content
Stress and Strain Cycling
Fatigue and Durability of Structural Materials
Introduction to Tensile Testing
Tensile Testing (Second Edition)
Significance of Mechanical Properties in Design and Application
Properties and Selection of Aluminum Alloys
201.0 and A201.0 Al-Cu High-Strength Premium Casting Alloys
Properties and Selection of Aluminum Alloys
Mechanical Work of Steels—Cold Working
Metallography of Steels Interpretation of Structure and the Effects of Processing
Characterization of Thermosetting Resins and Polymers
Characterization and Failure Analysis of Plastics
Mechanical Behavior of Materials under Tensile Loads
Tensile Testing (Second Edition)
Mechanical Testing
Metals Handbook Desk Edition (2nd Edition)
Plastic Deformation Structures
Metallography and Microstructures
Aluminum Alloy Temper Designations and Definitions
Properties and Selection of Aluminum Alloys