Chapter 7: Heat Treatment of Aluminum Castings
-
Published:2004
Abstract
The metallurgy of aluminum and its alloys offers a range of opportunities for employing heat treatments to obtain desirable combinations of mechanical and physical properties such that castings meet defined temper requirements. This chapter discusses the processes involved in solution heat treatment, quenching, precipitation hardening, and annealing of aluminum alloys. The effects of these processes on dimensional stability and residual stresses are also discussed. Troubleshooting and diagnosis of heat treating problems are covered in the concluding section of the chapter.
Sign in
ASM members
Member Sign InHeat Treatment of Aluminum Castings, Aluminum Alloy Castings: Properties, Processes, and Applications, By J. Gilbert Kaufman, Elwin L. Rooy, ASM International, 2004, p 61–68, https://doi.org/10.31399/asm.tb.aacppa.t51140061
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field