Chapter 6: Tribological Properties of Copper Alloys
-
Published:2021
Abstract
This chapter covers the friction and wear behaviors of copper alloys. It describes the compositions and forms of copper available and their suitability for applications involving friction, different types of erosion, and adhesive and abrasive wear.
You do not currently have access to this chapter.
Citation
Tribological Properties of Copper Alloys, Tribomaterials: Properties and Selection for Friction, Wear, and Erosion Applications, By Kenneth G. Budinski, Steven T. Budinski, ASM International, 2021, p 163–178, https://doi.org/10.31399/asm.tb.tpsfwea.t59300163
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.
Related Book Content
Tribological Properties of Cast Irons
Tribomaterials Properties and Selection for Friction, Wear, and Erosion Applications
Tribological Properties of Steels
Tribomaterials Properties and Selection for Friction, Wear, and Erosion Applications
Tribological Properties of Stainless Steel and Other Corrosion-Resisting Metals
Tribomaterials Properties and Selection for Friction, Wear, and Erosion Applications
Material Modifications (Coatings, Treatments, etc.) for Tribological Applications
Tribomaterials Properties and Selection for Friction, Wear, and Erosion Applications
Tribology of Plastics and Elastomers
Tribomaterials Properties and Selection for Friction, Wear, and Erosion Applications
Tribological Properties of Ceramics, Cermets, and Cemented Carbides
Tribomaterials Properties and Selection for Friction, Wear, and Erosion Applications
Metallurgy and Alloy Compositions
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Stress-Corrosion Cracking of Magnesium Alloys
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
2 xxx Aluminum Alloy Datasheets
Properties and Selection of Aluminum Alloys