This chapter provides a summary of ongoing efforts to improve quality and productivity in the aluminum extrusion industry. It assesses advancements in several areas including extrusion presses and auxiliary equipment, tool and die technology, billet casting, extrusion thermodynamics and tribology, and process control.
Topics
Extrusion
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Research and Development, Aluminum Extrusion Technology, By Pradip K. Saha, ASM International, 2000, p 245–248, https://doi.org/10.31399/asm.tb.aet.t68260245
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field
Related Book Content
List of Formula Symbols
Extrusion (Second Edition)
Thermodynamics in Extrusion
Aluminum Extrusion Technology
Extrusion Press and Auxiliary Equipment
Aluminum Extrusion Technology
Quality Management in Extrusion
Extrusion (Second Edition)
Approximate Composition of Materials
Extrusion (Second Edition)
Extrusion Die and Tooling
Aluminum Extrusion Technology
Process Control in the Aluminum Extrusion Plant
Aluminum Extrusion Technology
Statistical Process and Quality Control
Aluminum Extrusion Technology
Primary Working
Titanium Physical Metallurgy, Processing, and Applications
Glossary: Bulk Forming
Metalworking: Bulk Forming