This chapter covers the different types of extrusion presses in use, discussing their relative advantages, operating parameters, and selection factors. It describes the function of major components, including containers, stems, dummy pads, and die carriers, the maintenance they require, and their impact on productivity and the quality of extrusions. It also discusses the integration of auxiliary equipment such as log heaters and shears, quench systems, die ovens, pullers, stretchers, and stackers.