This chapter discusses the effect of fiber length and orientation on the strength and stiffness of discontinuous-fiber composites. It also describes several fabrication processes, including spray-up, compression molding, reaction injection molding, and injection molding.
You do not currently have access to this chapter.
Citation
Discontinuous-Fiber Composites, Structural Composite Materials, By F.C. Campbell, ASM International, 2010, p 285–305, https://doi.org/10.31399/asm.tb.scm.t52870285
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Composites
Elementary Materials Science
Compression Molding and Stamping
Engineered Materials Handbook Desk Edition
Bulk Molding Compounds
Engineered Materials Handbook Desk Edition
Compression Molding
Composites
Composite Structure Analysis
Optical Microscopy of Fiber-Reinforced Composites
Thermoplastic Composites Manufacturing
Composites
Electroformed Nickel Tooling
Composites
Design for Plastics Processing
Materials Selection and Design
Molding Compounds
Composites
Composite Structure Analysis
Metallography and Microstructures