Abstract
This chapter discusses the tooling used for autoclave curing, one of the most common composite fabrication processes. The discussion covers curing practices, material selection factors, and design challenges associated with thermal expansion, tool shrinkage, part complexity, and heating and cooling rates. The chapter also includes best practices and recommendations for toolmaking and assembly.
You do not currently have access to this chapter.
Citation
Fabrication Tooling, Structural Composite Materials, By F.C. Campbell, ASM International, 2010, p 101–118, https://doi.org/10.31399/asm.tb.scm.t52870101
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.
Related Book Content
Thermoplastic Composite Fabrication Processes
Structural Composite Materials
Introduction to Constituent Materials
Composites
Overview of Superalloys
Superalloys Alloying and Performance
Failure Analysis of a Polysulfone Flow Sensor Body — A Case Study
ASM Failure Analysis Case Histories: Failure Modes and Mechanisms
Low-Expansion Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
4 xxx Aluminum Alloy Datasheets
Properties and Selection of Aluminum Alloys
Thermomechanical Testing
Metalworking: Bulk Forming
Failure and Stress Analysis of Deformed Steel Tube
Handbook of Case Histories in Failure Analysis
336.0 Al-Si-Cu Permanent Mold Casting Alloy
Properties and Selection of Aluminum Alloys
Testing of Stability and Thermal Properties of Thermal Barrier Coatings
Surface Engineering