Chapter 14: Quality Control
-
Published:2015
Abstract
This chapter discusses quality control programs and procedures for induction heat-treating systems and includes related forms and checklists.
Topics
Hardness testing,
Induction furnaces,
Quenchants,
Quenching,
Induction surface hardening,
Case hardening,
Through hardening,
Induction tempering,
Hardenability,
Eddy current inspection,
Magnetic particle inspection,
Surface hardness,
Liquid penetrant inspection,
Ultrasonic inspection,
Inspection,
Qualification,
Statistical quality control,
Quality assurance and testing
You do not currently have access to this chapter.
Citation
Quality Control, Practical Induction Heat Treating, 2nd ed., By Richard E. Haimbaugh, ASM International, 2015, p 281–291, https://doi.org/10.31399/asm.tb.piht2.t55050281
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.
Related Book Content
Tempering
Practical Induction Heat Treating (Second Edition)
Induction Heat Treating Process Analysis
Practical Induction Heat Treating (Second Edition)
Quality Control and Quality Assurance
Steel Castings Handbook (Sixth Edition)
Process Control, Monitoring and Quality Assurance Specifics for Induction Heating
Induction Heating and Heat Treatment
Induction Hardening for the Aeronautic and Aerospace Industry
Induction Heating and Heat Treatment
Tempering of Induction Hardened Steels
Induction Heating and Heat Treatment
Crankshaft with Torsion Fatigue Fractures in Inductively Surface-Hardened Crank Pin
ASM Failure Analysis Case Histories: Improper Maintenance, Repair, and Operating Conditions
Induction Hardening Gears
Heat Treatment of Gears A Practical Guide for Engineers
Standards and Inspection
Practical Induction Heat Treating (Second Edition)
Localized Heat Treating
Metals Handbook Desk Edition (2nd Edition)