Abstract
This chapter discusses the quenching process and its adaptation to induction heat treating. It describes the three stages of quenching, the cooling characteristics of various types of quenchants, and the details of nearly a dozen compatible quenching methods. It also explains how to verify whether a quenchant can cool a workpiece fast enough to achieve martensitic transformation without cracking or distortion.
Topics
Hardness testing,
Induction furnaces,
Quenchants,
Quenching,
Induction surface hardening,
Case hardening,
Through hardening,
Induction tempering,
Hardenability,
Eddy current inspection,
Magnetic particle inspection,
Surface hardness,
Liquid penetrant inspection,
Ultrasonic inspection,
Inspection,
Qualification,
Statistical quality control
You do not currently have access to this chapter.
Citation
Quenching, Practical Induction Heat Treating, 2nd ed., By Richard E. Haimbaugh, ASM International, 2015, p 139–154, https://doi.org/10.31399/asm.tb.piht2.t55050139
Download citation file:
Related Book Content
Quenching with Molten Metal
Steel Heat Treating Technologies
Quenchant Agitation, Design, and Characterization
Steel Heat Treating Technologies
Quench Factor Characterization of Quenchants for Hardening of Steel
Steel Heat Treating Technologies
Transformation of Austenite and Quenching of Steel
Practical Heat Treating Basic Principles
Metallurgical Definitions for Induction Heat Treating
Practical Induction Heat Treating (Second Edition)
Design and Fabrication of Inductors for Induction Heat Treating
Induction Heating and Heat Treatment
Quenching of Induction Heated Steel
Induction Heating and Heat Treatment
Induction Heat Treating Systems
Practical Induction Heat Treating (Second Edition)
Nonconforming Product and Process Problems
Practical Induction Heat Treating (Second Edition)
Calculation of Heat Treating Costs
Steel Heat Treating Technologies