Chapter 2: Overview of Superalloys
-
Published:2010
Abstract
This chapter provides a brief overview of nickel-iron-base, cobalt-base, and nickel-base superalloys, discussing their basic metallurgy and defining characteristics.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Overview of Superalloys, Superalloys: Alloying and Performance, By Blaine Geddes, Hugo Leon, Xiao Huang, ASM International, 2010, p 9–15, https://doi.org/10.31399/asm.tb.sap.t53000009
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field
Related Book Content
Other Sources
Superalloys: A Technical Guide (Second Edition)
Introduction
Superalloys Alloying and Performance
Superalloys—Retrospect and Future Prospects
Superalloys: A Technical Guide (Second Edition)
Source Information
Superalloys: A Technical Guide (Second Edition)
Selected Superalloy Compositions
Superalloys Alloying and Performance
Superalloys for High Temperatures—a Primer
Superalloys: A Technical Guide (Second Edition)
Fabrication Tooling
Structural Composite Materials
Some Additional Microstructural Information
Superalloys: A Technical Guide (Second Edition)
Some Considerations in the Selection of a Superalloy
Superalloys Alloying and Performance
Selected Superalloy Properties
Superalloys Alloying and Performance