Abstract
This chapter discusses three related corrosion mechanisms, galvanic, deposition, and stray-current corrosion, explaining why they occur and how they affect the corrosion process. It includes information on testing and prevention methods along with examples of the type of damage associated with these corrosion mechanisms.
Topics
Aqueous corrosion,
Atmospheric corrosion,
Crevice corrosion,
Microbiologically-influenced corrosion,
Pitting corrosion,
Erosion corrosion,
Galvanic corrosion,
Intergranular corrosion,
Weld corrosion,
Stray current corrosion,
Corrosion fatigue,
Stress corrosion cracking,
Corrosion inhibitors,
Cast aluminum alloys,
Wrought aluminum alloys,
Aluminum alloys,
Anodizing,
Cladding,
Chromate conversion coating,
Plating,
Cleaning,
Alloy composition,
Corrosion testing,
Aluminum
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Galvanic, Deposition, and Stray-Current Corrosion, Corrosion of Aluminum and Aluminum Alloys, Edited By J.R. Davis, ASM International, 1999, p 75–83, https://doi.org/10.31399/asm.tb.caaa.t67870075
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!
Related Book Content
Stray-Current Corrosion
Corrosion in the Petrochemical Industry (Second Edition)
Corrosion of Aluminum and Aluminum Alloys
Corrosion: Materials
Pitting and Crevice Corrosion
Corrosion of Aluminum and Aluminum Alloys
External Corrosion of Oil and Natural Gas Pipelines
Corrosion in the Petrochemical Industry (Second Edition)
Effects of Metallurgical Variables on the Corrosion of Aluminum Alloys
Corrosion in the Petrochemical Industry (Second Edition)
U.S. Navy Aircraft Corrosion
Corrosion: Environments and Industries
Failure of Aluminum Alloy Spacers by Galvanic Attack
ASM Failure Analysis Case Histories: Failure Modes and Mechanisms
Summary of Aluminum Temper Designations
Aluminum Science and Technology
Laser Beam Machining of Aluminum and Aluminum Alloys
Aluminum Science and Technology
Chemical and Electrolytic Brightening
Aluminum Science and Technology