Abstract
This chapter describes the mechanisms, characteristics, and prevention of intergranular and exfoliation corrosion in various aluminum alloys. It discusses susceptible alloys and recommended tempers and presents several examples of exfoliation in aircraft components. It also explains how the two forms of corrosion are related to stress-corrosion cracking.
Intergranular and Exfoliation Corrosion, Corrosion of Aluminum and Aluminum Alloys, Edited By J.R. Davis, ASM International, 1999, p 63–74, https://doi.org/10.31399/asm.tb.caaa.t67870063