Chapter 13: Environmentally-Induced Failures
-
Published:2012
Abstract
This chapter discusses common forms of corrosion, including uniform corrosion, galvanic corrosion, pitting, crevice corrosion, dealloying corrosion, intergranular corrosion, and exfoliation. It describes the factors that contribute to stress-corrosion cracking, hydrogen embrittlement, and corrosion fatigue and compares and contrasts their effects on mechanical properties, performance, and operating life. It also includes information on high-temperature oxidation and corrosion prevention techniques.
Topics
Corrosion,
Damage tolerance assessment,
Deformation and fracture,
Manufacturing defects,
Fractography,
Wear,
Steel,
Fatigue testing,
Fracture resistance testing,
Threaded fasteners,
Aluminum alloys,
Stress rupture testing,
Titanium alloys,
Ceramics,
Tensile testing,
Polymers,
Brittleness,
Compressive properties,
Creep properties,
Elastic properties,
Fatigue properties,
Fracture toughness,
Shear and torsion properties,
Tensile properties,
Fatigue and fracture mechanics analysis,
Materials selection,
Fatigue life testing,
Fatigue analysis,
Crevice corrosion,
Pitting corrosion,
Dealloying corrosion,
Galvanic corrosion,
Intergranular corrosion,
Corrosion fatigue,
Stress corrosion cracking,
Uniform corrosion
You do not currently have access to this chapter.
Citation
Environmentally-Induced Failures, Fatigue and Fracture: Understanding the Basics, Edited By F.C. Campbell, ASM International, 2012, p 501–548, https://doi.org/10.31399/asm.tb.ffub.t53610501
Download citation file:
Related Book Content
Corrosion
Elements of Metallurgy and Engineering Alloys
Aqueous Corrosion Failures
Understanding How Components Fail (Third Edition)
Forms of Corrosion
Failure Analysis and Prevention (2021 Edition)
Forms of Corrosion: Recognition and Prevention
Corrosion: Understanding the Basics
Corrosion Control by Proper Design
Corrosion: Understanding the Basics
Automotive Body Corrosion
Corrosion: Environments and Industries
Forms of Corrosion
Failure Analysis and Prevention
Corrosion in Microelectronics
Corrosion: Environments and Industries
Engine Coolants and Coolant System Corrosion
Corrosion: Environments and Industries
Corrosion of Austenitic Stainless Steel Weldments
Corrosion of Weldments