Case 30: Failure of a Second-Stage Turbine Blade in an Aircraft Engine
-
Published:2005
Abstract
A second-stage turbine blade in an aircraft engine failed in service, fracturing along a path through the shroud hole. Cracks were also found in the shroud holes of the two adjacent blades. Based on the results of visual examination and SEM fractography, investigators concluded that the fracture and cracks were due to the fretting action of the pins inside the shroud holes.
Topics
Chemical analysis,
Corrosion,
Deformation and fracture,
Embrittlement,
Manufacturing defects,
Fractography,
Wear,
Aircraft components,
Fatigue testing,
Steam turbines,
Ball bearings,
Hardness testing,
Tensile testing,
Metallography,
Microscopy,
Nondestructive testing,
Aircraft landing gear,
Flight control and actuation systems,
Aircraft fuel system components,
Fuselage and wing structures,
Helicopter transmission systems,
Aircraft reciprocating engine components,
Aircraft turbine engine components,
Hydroturbines,
Bolts,
Screws,
Failure mode and effects analysis,
Root cause analysis,
Fretting wear,
Turbine blades,
Visual inspection
You do not currently have access to this chapter.
Citation
Failure of a Second-Stage Turbine Blade in an Aircraft Engine, Failure Analysis of Engineering Structures: Methodology and Case Histories, By V. Ramachandran, A.C. Raghuram, R.V. Krishnan, S.K. Bhaumik, ASM International, 2005, p 135–137, https://doi.org/10.31399/asm.tb.faesmch.t51270135
Download citation file:
Related Book Content
Failure of a Main Wheel Bearing Housing Flange in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Stabilizer Link Rod in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Wing Control Cable in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of an Adaptor Assembly in an Electronic Pod in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Tie-Rod in an Aircraft Towing Tractor
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Wheel Hub in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of Main Undercarriage Struts in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Low-Pressure Turbine Rotor (LPTR) Blade
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of Aircraft Engine Compressor Rotors
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a First-Stage Compressor Blade in an Aircraft Engine
Failure Analysis of Engineering Structures Methodology and Case Histories