Abstract
An adaptor and a bolt were overloaded during a flight causing them to fracture. This chapter recounts the circumstances that led to the failure and the investigation that followed. It includes images of the fracture surfaces which show that both components failed quickly due to overload conditions. It also recommends the use of twin suspension hooks to make attachment points more stable under difficult flight conditions.
Topics
Chemical analysis,
Corrosion,
Deformation and fracture,
Embrittlement,
Manufacturing defects,
Fractography,
Wear,
Aircraft components,
Fatigue testing,
Steam turbines,
Ball bearings,
Hardness testing,
Tensile testing,
Metallography,
Microscopy,
Nondestructive testing,
Aircraft landing gear,
Flight control and actuation systems,
Aircraft fuel system components,
Fuselage and wing structures,
Helicopter transmission systems,
Aircraft reciprocating engine components,
Aircraft turbine engine components,
Hydroturbines,
Bolts,
Screws,
Failure mode and effects analysis,
Root cause analysis,
Scanning electron microscopy,
Weapon systems,
Visual inspection
You do not currently have access to this chapter.
Citation
Failure of an Adaptor Assembly in an Electronic Pod in an Aircraft, Failure Analysis of Engineering Structures: Methodology and Case Histories, By V. Ramachandran, A.C. Raghuram, R.V. Krishnan, S.K. Bhaumik, ASM International, 2005, p 76–77, https://doi.org/10.31399/asm.tb.faesmch.t51270076
Download citation file:
Related Book Content
Failure of a Main Wheel Bearing Housing Flange in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Stabilizer Link Rod in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Wing Control Cable in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Tie-Rod in an Aircraft Towing Tractor
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Wheel Hub in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of Main Undercarriage Struts in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Second-Stage Turbine Blade in an Aircraft Engine
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of Aircraft Engine Compressor Rotors
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a First-Stage Compressor Blade in an Aircraft Engine
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Second-Stage Compressor Blade in an Aircraft Engine
Failure Analysis of Engineering Structures Methodology and Case Histories