Chapter 2: Common Causes of Failures
-
Published:2005
Abstract
This chapter identifies the primary causes of service failures and discusses the types of defects from which they stem. It presents more than a dozen examples of failures attributed to such causes as design defects, material defects, and manufacturing or processing defects as well as assembly errors, abnormal operating conditions, and inadequate maintenance. It also describes the precise usage of terms such as defect, flaw, imperfection, and discontinuity.
Topics
Chemical analysis,
Corrosion,
Deformation and fracture,
Embrittlement,
Manufacturing defects,
Fractography,
Wear,
Aircraft components,
Fatigue testing,
Steam turbines,
Ball bearings,
Hardness testing,
Tensile testing,
Metallography,
Microscopy,
Nondestructive testing,
Aircraft landing gear,
Flight control and actuation systems,
Aircraft fuel system components,
Fuselage and wing structures,
Helicopter transmission systems,
Aircraft reciprocating engine components,
Aircraft turbine engine components,
Hydroturbines,
Bolts,
Screws,
Failure mode and effects analysis,
Root cause analysis,
Ceramic insulators,
Pistons,
Shaft locking devices,
Elevators,
Failure mechanisms and analysis,
Turbine blades,
Beams and girders,
Cerclage wire,
Locomotive engine components
You do not currently have access to this chapter.
Citation
Common Causes of Failures, Failure Analysis of Engineering Structures: Methodology and Case Histories, By V. Ramachandran, A.C. Raghuram, R.V. Krishnan, S.K. Bhaumik, ASM International, 2005, p 5–17, https://doi.org/10.31399/asm.tb.faesmch.t51270005
Download citation file:
Related Book Content
Nonconforming Product and Process Problems
Practical Induction Heat Treating (Second Edition)
Products Liability and Design
Failure Analysis and Prevention
Products Liability and Design
Materials Selection and Design
Properties Needed for the Design of Static Structures
Materials Selection and Design
Failure of a Low-Pressure Turbine Rotor (LPTR) Blade
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Second-Stage Turbine Blade in an Aircraft Engine
Failure Analysis of Engineering Structures Methodology and Case Histories
Process Design for Induction Brazing and Soldering
Induction Heating and Heat Treatment
Premature Failure of a Turbine Blade by Thermal Fatigue Fracture
ASM Failure Analysis Case Histories: Air and Spacecraft
Failure of a Turbine Blade in an Aircraft Engine
Failure Analysis of Engineering Structures Methodology and Case Histories
Fractured Turbine Blades
ASM Failure Analysis Case Histories: Power Generating Equipment