Skip Nav Destination
ASM Technical Books
Inspection of Metals: Understanding the Basics
Edited by
ASM International
ISBN electronic:
978-1-62708-305-8
Publication date:
2013
Book Chapter
Chapter 9: Liquid Penetrant, Magnetic Particle, and Eddy-Current Inspection
-
Published:2013
Abstract
Liquid penetrant, magnetic particle, and eddy current inspection are used to detect surface flaws. This chapter is a detailed account of the physical principles, process description, equipment requirements, selection criteria, advantages, limitations, and applications of these surface flaw detection techniques.
Topics
Casting defects,
Surface flaws,
Welding defects,
Brinell hardness testing,
Rockwell hardness testing,
Knoop hardness testing,
Powder metal products,
Vickers hardness testing,
Bars,
Forgings,
Rods and wires,
Tubes,
Tensile testing,
Combustion analysis,
Metallography,
Forging,
Powder metallurgy,
Joint strength,
Eddy current inspection,
Stress-strain curves,
Magnetic particle inspection,
Industrial radiography,
Leak testing,
Coordinate measuring machines,
Liquid penetrant inspection,
Ultrasonic inspection,
Visual inspection,
X-ray fluorescence spectroscopy,
Optical emission spectroscopy,
Scanning Auger microscopes
You do not currently have access to this chapter.
Citation
Liquid Penetrant, Magnetic Particle, and Eddy-Current Inspection, Inspection of Metals: Understanding the Basics, Edited By F.C. Campbell, ASM International, 2013, p 183–232, https://doi.org/10.31399/asm.tb.imub.t53720183
Download citation file:
Related Book Content
Inspection of Tubular Products
Inspection of Metals Understanding the Basics
Inspection of Forgings
Inspection of Metals Understanding the Basics
Inspection of Weldments and Brazed Assemblies
Inspection of Metals Understanding the Basics
Inspection of Castings
Inspection of Metals Understanding the Basics
Inspection of Steel Bar and Wire
Inspection of Metals Understanding the Basics
Visual Inspection
Metals Handbook Desk Edition (2nd Edition)
Liquid Penetrant Inspection
Nondestructive Evaluation of Materials
Nondestructive Testing in Failure Analysis
Failure Analysis and Prevention (2021 Edition)