Nickel and Nickel Alloys
-
Published:2001
Abstract
This article examines the role of alloying in the production and use of nickel and its alloys. It explains how nickel-base alloys are categorized and lists the most common grades along with their compositional ranges and corresponding UNS numbers. It describes the role of nearly 20 alloying elements and how they influence strength, ductility, hardness, and corrosion resistance. It also addresses processing issues, explaining how alloying and intermetallic phases affect forming, welding, and machining operations.
Nickel and Nickel Alloys, Alloying: Understanding the Basics, Edited By J.R. Davis, ASM International, 2001, p 495–519, https://doi.org/10.31399/asm.tb.aub.t61170495