Metallography of Steels: Interpretation of Structure and the Effects of Processing
Chapter 13: Advanced Steels for Forming Operations
-
Published:2018
Abstract
This chapter discusses the properties and behaviors of advanced high-strength steels used in the automotive industry, including dual- and complex-phase steels, transformation-induced plasticity steels, ferritic-bainitic steels, and quenched and partitioned steels. It explains how different manufacturing processes, including coating, affect the grain size, microstructure, and formability of these important steels.
Sign in
ASM members
Member Sign InAdvanced Steels for Forming Operations, Metallography of Steels: Interpretation of Structure and the Effects of Processing, By Hubertus Colpaert;Edited By André Luiz V. da Costa e Silva, ASM International, 2018, p 445–474, https://doi.org/10.31399/asm.tb.msisep.t59220445
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field