Skip Nav Destination
ASM Technical Books
Elementary Materials Science
ASM International
ISBN electronic:
978-1-62708-283-9
Publication date:
2013
Book Chapter
Chapter 13: Forming and Shaping
-
Published:2013
Abstract
This chapter describes the processes, applications, and limitations of forming and shaping various materials. It discusses bulk forming, hot working, cold working, sheet forming, and polymer and powder processing.
You do not currently have access to this chapter.
Citation
Forming and Shaping, Elementary Materials Science, By William R. Hosford, ASM International, 2013, p 139–147, https://doi.org/10.31399/asm.tb.ems.t53730139
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.
Related Book Content
Design for Deformation Processes
Materials Selection and Design
Failures of Tools and Dies
Analysis and Prevention of Component and Equipment Failures
Fundamentals of Tribology in Metal Forming
Friction, Lubrication, and Wear Technology
Deformation Processing
Elements of Metallurgy and Engineering Alloys
Manufacturing Processes and Their Selection
Materials Selection and Design
Finite Element Method Applications in Bulk Forming
Metalworking: Bulk Forming
General Additives for Plastics and Elastomers
Engineered Materials Handbook Desk Edition
Design for Sheet Forming
Metalworking: Sheet Forming
Stress-Corrosion Cracking of Copper Alloys
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Powder Metallurgy Methods and Applications
Powder Metallurgy