Abstract
The die casting process is a widely applied technique used by a variety of industries. This chapter reviews the casting design and engineering requirements for optimizing the characteristics of die castings.
You do not currently have access to this chapter.
Citation
Engineering Die Castings, Aluminum Castings Engineering Guide, By Jagan Nath, ASM International, 2018, p 103–149, https://doi.org/10.31399/asm.tb.aceg.t68410103
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Sand Casting of Aluminum Alloys
Aluminum Science and Technology
Metal Waves or Laking on Zinc-Based Diecastings
ASM Failure Analysis Case Histories: Processing Errors and Defects
Intergranular Corrosion Failure in Zn-Al Alloy Solenoid Valve Seats
Handbook of Case Histories in Failure Analysis
Casting Design and Processes
Casting
Fatigue and Fracture Properties of Aluminum Alloy Castings
Fatigue and Fracture
Casting Design and Quality Assurance
Metals Handbook Desk Edition (2nd Edition)
Broken Full Lift Disk of a Safety Valve
ASM Failure Analysis Case Histories: Mechanical and Machine Components
Pattern Equipment
Steel Castings Handbook (Sixth Edition)
Plating Blemishes in Zinc Die Castings
ASM Failure Analysis Case Histories: Processing Errors and Defects
380.0, A380.0, and B380.0 General-Purpose Die-Casting Alloys
Properties and Selection of Aluminum Alloys