Abstract
This chapter examines methods of internal corrosion prediction for multiphase pipelines and details methodologies to perform internal corrosion direct assessment for natural gas pipelines. Further, real-time monitoring techniques for assessing actual corrosion at critical locations are discussed.
Topics
Atmospheric corrosion,
Gaseous corrosion,
Crevice corrosion,
Microbiologically-influenced corrosion,
Pitting corrosion,
Galvanic corrosion,
Weld corrosion,
Stray current corrosion,
Stress corrosion cracking,
Hydrogen embrittlement,
Carbon steel,
Stainless steel,
Corrosion inhibitors,
Chemical and petrochemical processing equipment,
Oil and gas refining equipment,
Nonferrous metals and alloys,
Corrosion,
Oil and gas pipelines
You do not currently have access to this chapter.
Citation
Natural Gas Internal Pipeline Corrosion, Corrosion in the Petrochemical Industry, 2nd ed., Edited By Victoria Burt, ASM International, 2015, p 349–359, https://doi.org/10.31399/asm.tb.cpi2.t55030349
Download citation file:
New Handbook: Volume 11B
Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.
Related Book Content
Galvanic Corrosion
Corrosion in the Petrochemical Industry (Second Edition)
Monitoring of Localized Corrosion
Corrosion: Fundamentals, Testing, and Protection