Corrosion in the Petrochemical Industry (Second Edition)
Abstract
This chapter presents the primary considerations and mechanisms for corrosion and how they are involved in the selection of materials for process equipment in petroleum refineries and petrochemical plants. In addition, specific information on mechanical properties, corrosion, sulfide stress cracking, hydrogen-induced cracking, stress-oriented hydrogen-induced cracking, hydrogen embrittlement cracking, stress-corrosion cracking, velocity-accelerated corrosion, erosion-corrosion, and corrosion control is provided.
Corrosion in Petroleum Refining and Petrochemical Operations, Corrosion in the Petrochemical Industry, 2nd ed., Edited By Victoria Burt, ASM International, 2015, p 292–337, https://doi.org/10.31399/asm.tb.cpi2.t55030292
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.