Abstract
This chapter describes the effects of metallurgical variables on the corrosion of aluminum alloys. Emphasis is placed on the effect of constituent particles on pitting corrosion of aluminum.
Topics
Atmospheric corrosion,
Gaseous corrosion,
Crevice corrosion,
Microbiologically-influenced corrosion,
Pitting corrosion,
Galvanic corrosion,
Weld corrosion,
Stray current corrosion,
Stress corrosion cracking,
Hydrogen embrittlement,
Carbon steel,
Stainless steel,
Corrosion inhibitors,
Chemical and petrochemical processing equipment,
Oil and gas refining equipment,
Nonferrous metals and alloys,
Corrosion,
Aluminum alloys,
Aluminum
You do not currently have access to this chapter.
Citation
Effects of Metallurgical Variables on the Corrosion of Aluminum Alloys, Corrosion in the Petrochemical Industry, 2nd ed., Edited By Victoria Burt, ASM International, 2015, p 70–73, https://doi.org/10.31399/asm.tb.cpi2.t55030070
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.
Related Book Content
Effects of Metallurgical Variables on the Corrosion of Aluminum Alloys
Corrosion: Fundamentals, Testing, and Protection
Summary of Aluminum Temper Designations
Aluminum Science and Technology
Laser Beam Machining of Aluminum and Aluminum Alloys
Aluminum Science and Technology
Chemical and Electrolytic Brightening
Aluminum Science and Technology
Aluminum—The Light Metal
The History of Metals in America
Understanding the Corrosion Behavior of Aluminum
Corrosion of Aluminum and Aluminum Alloys
Types of Corrosive Environments
Corrosion of Aluminum and Aluminum Alloys
Chemical Compositions and International Designations for Aluminum Alloys
Metals Handbook Desk Edition (2nd Edition)
Etching of Aluminum and Its Alloys
Aluminum Science and Technology
Introduction
Corrosion of Aluminum and Aluminum Alloys