Abstract
This article reviews fatigue test methodologies, provides an overview of general fatigue behavior (crack initiation and propagation) in engineering plastics, and discusses some of the factors affecting the fatigue performance of polymers. In addition, it provides information on fractography that provides useful insight into the nature of fracture processes.
You do not currently have access to this chapter.
Citation
Fatigue Testing and Behavior, Characterization and Failure Analysis of Plastics, Edited By Steven Lampman, ASM International, 2003, p 238–248, https://doi.org/10.31399/asm.tb.cfap.t69780238
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.
Related Book Content
Malleable Irons/White Irons: Atlas of Fractographs
Fractography
Mechanisms of Stress-Corrosion Cracking
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Stress-Corrosion Cracking
Corrosion in the Petrochemical Industry (Second Edition)
Stress-Corrosion Cracking
Corrosion: Fundamentals, Testing, and Protection
Fatigue Failure
Characterization and Failure Analysis of Plastics
Fracture and Fractography
Characterization and Failure Analysis of Plastics
Failure of a First-Stage Compressor Blade in an Aircraft Engine
Failure Analysis of Engineering Structures Methodology and Case Histories
Fatigue Strength of Metals
Mechanics and Mechanisms of Fracture An Introduction
Fracture of Plastics
Characterization and Failure Analysis of Plastics