Chapter 14: Design Guidelines for Advanced High-Strength Steels
-
Published:2013
Abstract
This chapter briefly reviews the experience-based guidelines that were developed for forming and welding advanced high-strength steels (AHSS). It discusses the benefits of using HSS in car body structures and components that are analyzed by the performance indices developed for materials selection.
You do not currently have access to this chapter.
Citation
Design Guidelines for Advanced High-Strength Steels, Advanced-High Strength Steels: Science, Technology, and Applications, By Mahmoud Y. Demeri, ASM International, 2013, p 215–224, https://doi.org/10.31399/asm.tb.ahsssta.t53700215
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Consequences of Using Advanced High-Strength Steels
Advanced-High Strength Steels Science, Technology, and Applications
Forming of Advanced High-Strength Steels
Metalworking: Sheet Forming
Innovative Forming Technologies
Advanced-High Strength Steels Science, Technology, and Applications
Forming of Steel Tailor-Welded Blanks
Metalworking: Sheet Forming
Performance Indices
Materials Selection and Design
Nickel and Nickel Alloys
Alloying Understanding the Basics
Introduction
Advanced-High Strength Steels Science, Technology, and Applications
Applications of Advanced High-Strength Steels
Advanced-High Strength Steels Science, Technology, and Applications
Global Projects on Advanced High-Strength Steels
Advanced-High Strength Steels Science, Technology, and Applications
Evolving Advanced High-Strength Steel Grades
Advanced-High Strength Steels Science, Technology, and Applications