Chapter 7: Transformation-Induced Plasticity Steels
-
Published:2013
Abstract
Transformation-induced plasticity (TRIP) steels are characterized by their excellent strength and high ductility, which allow the production of more complicated parts for lightweight automotive applications. This chapter provides an overview of the compositions, microstructures, processing, deformation mechanism, mechanical properties, hot forming, tempering, and special attributes of TRIP the steels.
Transformation-Induced Plasticity Steels, Advanced-High Strength Steels: Science, Technology, and Applications, By Mahmoud Y. Demeri, ASM International, 2013, p 115–125, https://doi.org/10.31399/asm.tb.ahsssta.t53700115