Chapter 6: Complex-Phase Steels
-
Published:2013
Abstract
This chapter provides an overview of the composition, microstructures, processing, deformation mechanism, mechanical properties, formability, and special attributes of complex-phase steels.
You do not currently have access to this chapter.
Citation
Complex-Phase Steels, Advanced-High Strength Steels: Science, Technology, and Applications, By Mahmoud Y. Demeri, ASM International, 2013, p 107–113, https://doi.org/10.31399/asm.tb.ahsssta.t53700107
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.
Related Book Content
Dual-Phase Steels
Advanced-High Strength Steels Science, Technology, and Applications
Twinning-Induced Plasticity Steels
Advanced-High Strength Steels Science, Technology, and Applications
Austenitic Stainless Steels
Advanced-High Strength Steels Science, Technology, and Applications
Steel Fundamentals
Advanced-High Strength Steels Science, Technology, and Applications
Transformation-Induced Plasticity Steels
Advanced-High Strength Steels Science, Technology, and Applications
Martensitic Steels
Advanced-High Strength Steels Science, Technology, and Applications
Alteration of Microstructure
Metallographer’s Guide Practices and Procedures for Irons and Steels
Nanofluids as Quenchants in Industrial Heat Treatment
Steel Heat Treating Technologies
Heat Treating of Magnesium Alloy Metal-Matrix Composites
Heat Treating of Nonferrous Alloys
Design for Deformation Processes
Materials Selection and Design