Chapter 5: Dual-Phase Steels
-
Published:2013
Abstract
Dual-phase (DP) steels have the widest usage in automotive industry because of their excellent combination of strength and ductility. This chapter provides an overview of the composition, microstructure, processing, deformation mechanism, mechanical properties, formability, and special attributes of DP steels.
You do not currently have access to this chapter.
Citation
Dual-Phase Steels, Advanced-High Strength Steels: Science, Technology, and Applications, By Mahmoud Y. Demeri, ASM International, 2013, p 95–106, https://doi.org/10.31399/asm.tb.ahsssta.t53700095
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Twinning-Induced Plasticity Steels
Advanced-High Strength Steels Science, Technology, and Applications
Austenitic Stainless Steels
Advanced-High Strength Steels Science, Technology, and Applications
Complex-Phase Steels
Advanced-High Strength Steels Science, Technology, and Applications
Dual-Phase Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Steel Fundamentals
Advanced-High Strength Steels Science, Technology, and Applications
Transformation-Induced Plasticity Steels
Advanced-High Strength Steels Science, Technology, and Applications
Martensitic Steels
Advanced-High Strength Steels Science, Technology, and Applications
Alteration of Microstructure
Metallographer’s Guide Practices and Procedures for Irons and Steels
Nanofluids as Quenchants in Industrial Heat Treatment
Steel Heat Treating Technologies
Heat Treating of Magnesium Alloy Metal-Matrix Composites
Heat Treating of Nonferrous Alloys