Chapter 2: Steel Fundamentals
-
Published:2013
Abstract
This chapter discusses the compositions, metallurgical phases, microstructure, heat treatment, grades, and structure-property relationships of steels. In addition, it describes the mechanisms involved in deformation, strengthening, and annealing of steels.
You do not currently have access to this chapter.
Citation
Steel Fundamentals, Advanced-High Strength Steels: Science, Technology, and Applications, By Mahmoud Y. Demeri, ASM International, 2013, p 23–58, https://doi.org/10.31399/asm.tb.ahsssta.t53700023
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Dual-Phase Steels
Advanced-High Strength Steels Science, Technology, and Applications
Twinning-Induced Plasticity Steels
Advanced-High Strength Steels Science, Technology, and Applications
Austenitic Stainless Steels
Advanced-High Strength Steels Science, Technology, and Applications
Complex-Phase Steels
Advanced-High Strength Steels Science, Technology, and Applications
Alteration of Microstructure
Metallographer’s Guide Practices and Procedures for Irons and Steels
Structure/Property Relationships in Irons and Steels
Metals Handbook Desk Edition (2nd Edition)
Cyclic Stress-Strain Response and Microstructure
Fatigue and Fracture
Mechanisms and Causes of Failures in Heat Treated Steel Parts
Failure Analysis of Heat Treated Steel Components
Deformation, Mechanical Properties, and Fracture of Quenched and Tempered Carbon Steels
Steels: Processing, Structure, and Performance (Second Edition)
Transformation-Induced Plasticity Steels
Advanced-High Strength Steels Science, Technology, and Applications